Hands Off Hartlebury Common

Steve McCarron

/ #1173 Re:

2011-07-25 15:59

#1171: -

Were not selling any at the moment, not because we are not getting enquires but because we use Aluminium Bronze CA104

Our local casting company originally supplied us  castings in the above material. However as good as CA104 is (it looks like gold when finished) we were faced with an unacceptable degree of porosity and therefore scrap castings. Rather than cast in another metal, we have put things on hold indefinatley until we can redress this issue. Our cutlery graces some of the finest dining tables in the country.


Case not proven and far from resolved. I can think of two schemes where the public finally had these schemes stopped. It was not easy but it happened. It was decided after 10 years that the experiment had failed in both.

The landscape was ruined, see below.